Previous Product Next Product Numerical modelling of electron beam welding (EBW) of Zhs6u superalloy and its experimental validation ₩4,000 Numerical modelling of electron beam welding (EBW) of Zhs6u superalloy and its experimental validation 수량 장바구니 카테고리: 과학기술 정보 (유료), 러시아 및 CIS 국가 과학기술정보 상품평 (0) 상품평 아직 상품평이 없습니다. “Numerical modelling of electron beam welding (EBW) of Zhs6u superalloy and its experimental validation”의 첫 상품평을 남겨 주세요 응답 취소상품평 작성을 위해 로그인이 필요합니다. 연관 상품 Quick View Feedback system could help to correct errors in quantum computersLog in to view price and purchase Quick View Quantum nanodevice can be both a heat engine and a fridge at the same timeLog in to view price and purchase Quick View Simulating spins, spirals and shrinking devicesLog in to view price and purchase