Previous Product Next Product Role of shrinkage pores, carbides on cyclic deformation behaviour of conventionally cast nickel base superalloy CM247LC at 870 °C ₩4,000 Role of shrinkage pores, carbides on cyclic deformation behaviour of conventionally cast nickel base superalloy CM247LC at 870 °C 수량 장바구니 카테고리: 과학기술 정보 (유료), 러시아 및 CIS 국가 과학기술정보 상품평 (0) 상품평 아직 상품평이 없습니다. “Role of shrinkage pores, carbides on cyclic deformation behaviour of conventionally cast nickel base superalloy CM247LC at 870 °C”의 첫 상품평을 남겨 주세요 응답 취소상품평 작성을 위해 로그인이 필요합니다. 연관 상품 Quick View A new, sustainable way to make hydrogen for fuel cells and fertilizersLog in to view price and purchase Quick View Mott insulator exhibits a sharp response to electron injectionLog in to view price and purchase Quick View Feedback system could help to correct errors in quantum computersLog in to view price and purchase